含Cl-大气对铝、铜、锌、18-8不锈钢的腐蚀及防腐措施
The Corrosion of Aluminum, Copper, Zinc & 18-8 Stainless Steel Caused by Air Contained Clˉ& Protecting Measures
浏览(1685) 下载(1)
- DOI:
- 作者:
- 王国清, 赵旭, 李鹏
Wang Guoqing
- 作者单位:
- 塔里木石化工程建设指挥部
- 关键词:
- 有色金属;不锈钢;大气腐蚀;基层处理;表面涂装
non-ferrous metal;stainless steel;atmosphere corrosion;matrix treatment;surface coating
- 摘要:
- 针对塔里木石化厂有色金属和 18-8不锈钢受大气中有害气体腐蚀的实际情况,通过对大气取样分析和金属挂片试验,确定了其腐蚀等级,分析了含Cl-大气对铝、铜、镀锌板等有色金属及 18-8不锈钢的腐蚀机理,并提出了防腐处理措施,包括金属表面处理、涂料的选择和涂敷
In connection with that the actual situation of non-ferrous metal 18-8 stainless steel were corroded by the air contained harm gas, through sampling analyzing to the air and metal hanging sheet test, the writers determine their corrosion grade, analyze the mechanism of aluminum, copper, galvanized iron sheet etc. non-ferrous metal 18-8 stainless steel corrosion caused by air contained Clˉ and puts forward some anti-corrosion measures including metal surface treatment, paints selecting coating method.2002,6(6): 35-37,3,4 收稿日期:2002-7-4分类号:TG174作者简介:王国清,高级工程师,中国腐蚀与防护协会会员.1986年毕业于河南化工学校化机专业,1996年毕业于河南财经学院经济管理专业.十几年来一直从事防腐蚀技术和设备维修技术的管理工作,已发表论文5篇.通讯地址:新疆库尔勒市132信箱,邮编:841000参考文献:
[1]虞兆年.防腐蚀涂料和涂装.北京:化学工业出版社,2002
[2]SH3022-1999石油化工设备和管道涂料防腐蚀技术规范
[3]李祉川等.化工设备的维护检修.北京:化学工业出版社,1989
[4]余成(钅昌),刘伯英.化工厂设备管理.北京:化学工业出版社,1984
[5]楼宇新.化工机械制造工艺与安装修理.北京:化学工业出版社,1984