大型外浮顶储罐浮盘底板焊缝正压试验技术
Positive Pressure Leakage Test Technique for Bottom Plate Welds of Large Scale External Floating Roof Tank
浏览(2263) 下载(2)
- DOI:
- 作者:
- 李剑平1, 杨贝斌2, 李春辉1, 岳实全1
LI Jian-ping1
- 作者单位:
- 1. 新疆吐哈油田建设有限责任公司, 新疆吐鲁番 838202;
2. 新疆吐哈油田公司工程质量监督站, 新疆吐鲁番 838202
Xinjiang Tuha Oilfield Construction Co., Ltd., Tulufan 838202, China
- 关键词:
- 大型外浮顶储罐;浮盘底板渗漏;正压试验;真空箱试漏法;应用
large scale external floating roof;tankleakage at bottom plate of floating roof;leakage test;with vacuum;chamberapplication
- 摘要:
- 文章结合工程实际,在分析了大型外浮顶储罐浮盘底板出现渗漏原因的基础上,指出了浮盘底板焊缝传统的真空箱试漏法存在的缺陷和不足,并根据储罐浮盘底板焊缝的结构特点,提出了新的焊缝正压试验法来弥补传统试验方法的不足。工程应用表明,新试验方法试漏效果良好。
Based on the reason analysis of leakage at floating roof bottom plates of a large scale external floating roof tank,the deficiency and shortcoming of traditional leakage test with vacuum chamber are pointed out.According to structural characteristics of the welds at floating roof bottom plates,a new weld leakage test method,i.e.positive pressure leakage test method,is put forward to remedy the traditional method.The engineering practice shows that the new leakage test method works well.2010,6(6): 59-60 收稿日期:2010-1-27分类号:TE972.5作者简介:李剑平(1969-),男,安徽凤台人,工程师,1998年毕业于西南石油大学矿场机械专业,一直从事石油化工项目建设工作.