储罐横向埋弧自动焊焊缝裂纹的防治措施
Prevention and Treatment of Weld Cracks at Storage Tank Occurred in Transverse ArcAutomatic Welding
浏览(2508) 下载(7)
- DOI:
- 作者:
- 刘瑞祥, 张德文, 程铁军, 郎建春
LIU Rui-xiang
- 作者单位:
- 中国石油天然气管道局第二工程分公司, 江苏徐州 221008
No.2 Subsidiary Construction Company of China Petroleum Pipeline Bureau,Xuzhou 221008,China
- 关键词:
- 储罐;横焊;环缝;焊接;热裂纹;防治
storage tank;transverse welding;circular seam;heating crack;prevention and treatment
- 摘要:
- 储罐的焊接裂纹多数发生在横向埋弧自动焊的焊接过程中,文章分析了裂纹产生的原因,提出了控制裂纹的几项措施,并对裂纹的检验和处理进行了说明。
Weld cracks at storage tanks occur mostly in the process of transverse submerged arc automaticwelding. By linking theory with practice,the authors came to discover some laws why the cracks formed andhow to prevent them, then put forward several measures to control the cracks and some methods for crack in-spection and treatment.2010,2(2): 44-46 收稿日期:2009-2-17分类号:TU972作者简介:刘瑞祥(1962-),男,河北肃宁人,高级工程师,1987年毕业于华北石油职工大学工民建专业,现从事储罐施工技术工作.?